When a customer sends over a die casting drawing, the first thing I check is wall thickness uniformity. In die casting, uneven walls are a recipe for trouble: thick sections cool slower than thin ones, creating shrinkage porosity and hot spots that show up as defects after machining. A good rule of thumb is to keep nominal wall thickness in the 1.5–3.0 mm range for aluminum alloys, and where thickness must change, transition gradually rather than stepping abruptly. On the mold side, this directly affects die life—thermal fatigue cracking concentrates at thickness transitions, and I have seen dies fail at those spots well before reaching expected cycle counts. If a design demands a thick boss or rib junction, plan for a cooling insert or jet cooling in that area of the die rather than hoping the problem away.

Fillets and draft angles are the next items on my checklist. Sharp internal corners act as stress risers on the casting and as heat concentrators on the die; a minimum internal fillet radius of 0.5–1.0 mm, scaled up with wall thickness, is standard practice. External corners should carry a radius too, typically equal to the internal fillet plus the wall thickness, to keep metal flow smooth during filling. Draft angles matter just as much for ejection: 1–2 degrees on vertical walls is typical, with 2–3 degrees on deeper cores or textured surfaces. Insufficient draft leads to galling, sticking, and ejector pin marks—problems that get blamed on the mold but usually originate in the part design. When we quote a die, draft and fillet quality directly influence how much polishing and spotting labor goes into the tool.

Finally, don't overlook features like ribs, bosses, and cored holes. Ribs should be thinner than the adjoining wall—roughly 0.5–0.7 times wall thickness—to avoid sinking on the opposite surface, and bosses need supporting ribs or gussets rather than standing alone. Cored holes smaller than about 2 mm in diameter are risky for pins that see repeated thermal cycling. Getting these details right at the design stage saves weeks of tool rework later. For more mold sourcing and die casting supplier information, visit MoldSo at www.moldso.com.