In stamping, the press and die apply force to sheet, strip, tube or profile stock to cause plastic deformation or separation, giving the part its required shape and size. For the die engineer, the whole game usually comes down to clearance and how it matches the material. Blanking clearance is typically 5% to 10% of stock thickness โ€” run it on the small side for soft materials and on the large side for hard ones. Get the clearance wrong and you will see burrs, collapse and secondary shear at the cut edge, which means rework on the die and scrap on the floor. In our shop, we check clearance per station after the first trial run rather than trusting the drawing alone, because actual material thickness tolerance shifts the effective number.

Drawing adds another layer of control. Blankholder force and drawing coefficient have to be balanced: for carbon steel the first draw coefficient is roughly 0.5 to 0.6. Too much blankholder force and the part tears; too little and it wrinkles. We adjust the cushion pressure in small steps during tryout and record the setting per material lot, since incoming coil hardness varies. Die steel selection matters just as much for service life. Blanking dies commonly use Cr12MoV, while drawing dies are often built from SKD11 with TD coating โ€” in practice this can extend die life by 3 to 5 times, which pays back quickly on high-volume runs.

None of this is theoretical on the shop floor. Clearance, blankholder force and die material have to be tuned together for each job, and the trial run is where that happens. Keep records of what worked per material and thickness, and the next die build starts from a known baseline instead of guesswork. For more mold sourcing information, visit MoldSo at www.moldso.com.