When I review a die casting part drawing, the first thing I check is wall thickness. Uniform walls are the single biggest factor in avoiding shrinkage porosity and cold shuts, and in practice most zinc and aluminum die castings should stay in the 1.5–3.0 mm range for the main walls, with thin sections not dropping below roughly 0.8 mm unless the alloy and gating are carefully engineered. Where thickness has to change, I want gradual transitions — a step of no more than 1:3 taper between adjacent sections — because abrupt jumps create isolated hot spots that pull shrinkage defects right where the part needs strength. Ribs should be thinner than the adjoining wall, typically 0.5–0.7 times the wall thickness, and kept shallow with generous fillets; that way they stiffen the part without feeding a thick node at the intersection.
Draft angle is the other point I refuse to compromise on. On cored features and deep pockets, a minimum of 1–2 degrees per side is standard practice, and for textured surfaces you need to add 1 degree or more on top of the base draft to keep ejection clean. Sharp internal corners are crack starters in the die steel as well as stress risers in the casting, so I call for fillets of at least 0.5 mm internal radius, larger at parting-line intersections. Ejector pin locations, gate vestiges, and overflow positions all need to be agreed with the toolmaker at the design stage — not after the cavity is cut — because moving a gate later means welding and re-sparking a die block, and that costs real money and lead time.
The last thing I tell every product designer: design for the die, not just for the assembly. Put the parting line where it can be machined flat, keep slides and lifters to a minimum, and specify tolerances that match what high-pressure die casting can actually hold — typically around ±0.05 mm on critical features before secondary machining. Get these fundamentals right at the drawing stage and the tool build, trial shots, and production all get cheaper. For more mold sourcing and supplier information, visit MoldSo at www.moldso.com.
We run a lot of aluminum enclosures for LED drivers, and wall thickness is where projects die. Had one at 1.2mm nominal that looked fine on the drawing but flashed at the parting line once tooling wore in. We bumped to 1.8mm and added 1.5 degree draft on the deep pockets. Tooling cost went up maybe 8 percent but scrap dropped from 6 percent to under 2. Cheaper in the long run.