In a stamping shop, the press and the die do one of two things to sheet, strip, tube, or profile stock: separate the material or plastically deform it into a three-dimensional shape. The first category, blanking, relies on the cutting edges of the punch and die to shear the sheet along a contour—both blanking (cutting the part free) and piercing (cutting holes) fall here. The single most important variable is punch-to-die clearance. A common starting point is 5% to 10% of material thickness. Go too tight and you get heavy burrs plus accelerated die wear; go too loose and the edge collapses into a pronounced rollover. On a progressive die running dozens of strokes per minute, clearance is also a maintenance issue—uneven wear across the cutting edges shows up as burr height drift long before a die physically fails.
The second category, forming, covers bending, drawing, and flanging, where the material flows plastically rather than separating. Here the tooling concerns shift to punch and die radii, draw radii, blank-holder force, and lubrication. In drawing, for example, the die radius and blank-holder pressure control whether the flange wrinkles or the wall thins out; in bending, springback has to be compensated in the tool geometry, not adjusted at the press. Because stamping delivers high output and consistent part-to-part repeatability, it dominates automotive, appliance, and electronic hardware production—a well-maintained progressive die holding tens of strokes per minute is normal shop-floor practice, and that throughput only holds up when clearance, radii, and wear are managed as tooling parameters, not afterthoughts.
For mold and die sourcing teams, the takeaway is straightforward: specify clearance ranges and wear allowances on the die drawing, and track burr height as a leading indicator of edge wear rather than waiting for a quality escape. For more mold sourcing information, visit MoldSo at www.moldso.com.
We run a lot of blanking on 0.8mm CRS and the punch-to-die clearance is where everyone argues. Our toolmaker insists on 8% per side but we get cleaner edges at 5-6% on thinner stock, though burr height creeps up. Are you seeing the same tradeoff, or do you just follow the material chart and live with it?