Every die casting quote starts with the part drawing, and the first thing I check is wall thickness. Thin walls cool fast and fill poorly; thick walls bring shrinkage porosity that no amount of shot pressure fully fixes. In practice, zinc alloys run comfortably at 0.6–1.5 mm, while aluminum sits around 1.5–3.0 mm, with 2.5 mm being a safe default for structural housings. Where a boss or rib meets the main wall, keep the thickness ratio near 0.6–0.7 to avoid hot spots and sink. Uniform wall sections also shorten cycle time and reduce die thermal fatigue — a point that matters when the tool is expected to run 100,000+ shots.
Draft angle is the second item on my checklist. Inside walls need at least 1–2°, outside walls 0.5–1°, and textured surfaces demand more — roughly 1.5° extra per 0.025 mm of texture depth. Skip this and you get drag marks, ejection distortion, or a part that sticks and cracks at the ejector pins. Corner radii should be generous: internal fillets of at least 0.5× wall thickness reduce stress concentration and improve metal flow. Ribs should be thinner than the wall they reinforce, with a draft on both sides, and bosses should be tied to nearby walls with gussets rather than standing alone. These details directly affect die cost — a part designed with proper draft and fillets often needs fewer slides and a simpler tool.
Then comes the shop-floor reality: gate location, overflow placement, and ejector pin layout all depend on the part geometry you hand over. A design that ignores parting line constraints will come back as a quote with extra slides, more machining, and a longer lead time. Before releasing a drawing, sit with the die caster and walk through fill simulation, shrinkage allowance (typically 0.4–0.6% for aluminum), and machining stock. For more mold sourcing and die casting supplier information, visit MoldSo at www.moldso.com.
We used to run a 2.0mm wall on an A380 aluminum housing and kept getting cold shuts at the far end of the cavity until we bumped the wall to 2.5mm and slowed the fill. Cheaper than fighting porosity and X-ray rejects. Curious how you handle draft on deep ribs—we're at 1.5 degrees and still dragging on ejection.